PSD-GOLD activated carbon product

PSD-GOLD | Coconut Shell Carbon for Gold Recovery (CIP/CIL/CIC)

Engineered for maximum gold recovery with minimal carbon loss. PSD-GOLD is a high-hardness coconut shell activated carbon optimized for CIP, CIL, and CIC circuits—delivering rapid aurocyanide adsorption, low attrition, and multi-cycle regenerability for mining operations worldwide.

Share:

Applications:

Product Overview

PSD-GOLD is a premium coconut shell granular activated carbon engineered specifically for the rigorous demands of precious metal recovery circuits. Manufactured from dense, mature coconut shells selected for high lignin content, this carbon delivers the robust granular structure required to withstand the abrasive conditions of carbon-in-pulp (CIP), carbon-in-leach (CIL), and carbon-in-column (CIC) gold extraction processes.

In gold recovery, carbon fines are silent profit killers. Every gram of carbon dust escaping interstage screens carries adsorbed gold into tailings. PSD-GOLD's >98% hardness—the highest in the coconut shell range—drastically reduces fines generation, cutting gold losses and simplifying tailings management. Combined with a micropore structure tuned for rapid aurocyanide complex adsorption, it achieves competitive gold loadings while maintaining structural integrity through repeated thermal reactivation cycles.

Key Application Areas

  • Gold Recovery — CIP/CIL/CIC Processes: Purpose-built for carbon-in-pulp, carbon-in-leach, and carbon-in-column gold extraction circuits, delivering high gold loading capacity and rapid adsorption kinetics in slurry and solution-phase operations
  • Precious Metal Refining: Efficient recovery of silver, platinum group metals, and other precious metals from leach solutions and electroplating effluents through selective adsorption
  • Mining Operations: Robust performance in large-scale heap leach and agitated leach mining operations where carbon attrition resistance and mechanical strength are critical for minimizing gold losses
  • Carbon Regeneration Circuits: Engineered for repeated thermal reactivation cycles, maintaining >90% capacity recovery after regeneration to reduce operating costs in high-volume gold processing plants
  • Tailings & Wastewater Treatment: Recovery of residual precious metals from tailings streams and process wastewater, supporting environmental compliance and resource maximization

Specifications

Technical SpecificationsPSD-GOLDUnit
CTC Number50 min%
Iodine Number 1050 minmg/g
Total Ash Content5 max%
Moisture10 max%
Hardness98 min%
Apparent Density0.45-0.54g/cc
Particle Size6-12mesh

Available particle size

  • 6×12 Mesh
  • 4×8 Mesh

Packaging

  • The 20 kg / Package
  • The 500 kg / Package

Key Performance Metrics

  • Superior Gold Loading Capacity: The micropore structure is tuned for aurocyanide complex adsorption, achieving loadings that compete with the best mining carbons globally
  • Exceptional Hardness & Low Fines Generation: 98% minimum hardness means less carbon loss per cycle—translating to lower make-up carbon costs and cleaner tailings
  • Fast Adsorption Kinetics: The pore size distribution favors fast mass transfer, ensuring gold is captured before it exits the circuit
  • Multi-Cycle Thermal Regenerability: Thermal reactivation restores capacity efficiently, with minimal structural degradation over multiple cycles

How PSD-GOLD Achieves Coconut Shell Carbon Gold Recovery

Gold recovery from cyanide leach solutions depends on rapid aurocyanide complex adsorption and high gold loading capacity per unit volume. In the abrasive slurry environments of CIP/CIL/CIC circuits, standard carbons with lower hardness generate excessive fines during interstage screening and carbon transfer, carrying gold losses to tailings and complicating tailings management.

  • Raw Material Selection: Dense, mature coconut shell selection with high lignin content is the foundation of PSD-GOLD. The robust granular structure withstands the mechanical stress of continuous slurry pumping, screening, and elution cycling.
  • Micropore Engineering for Gold Capture: The micropore architecture is tuned for rapid aurocyanide complex adsorption, achieving competitive gold loadings with fast mass transfer kinetics that capture dissolved gold before it exits the circuit.
  • Hardness That Pays Back: The >98% hardness is the highest in the coconut shell range, directly translating to lower carbon makeup rates and reduced gold losses. The pore structure also supports efficient thermal reactivation, restoring capacity for multiple cycles with minimal structural degradation.

Why Choose PSD-GOLD?

Unlike tolling-dependent suppliers, PureStar operates four integrated production facilities with full control from raw material selection to steam activation. Every batch of PSD-GOLD undergoes rigorous hardness and iodine testing to ensure consistent performance in high-abrasion mining circuits. With flexible packaging and technical support for circuit optimization, we deliver not just carbon—but a reliable recovery partner.

Why Mining-Grade Coconut Shell Carbon Matters

Not all activated carbon performs equally in abrasive CIP/CIL slurry environments. Peat-based and wood-based carbons, while lower in initial cost, suffer from higher attrition—their softer structures generate excessive fines during interstage screening and carbon transfer, carrying adsorbed gold into tailings and inflating carbon makeup costs.

Standard coconut shell carbons offer better hardness, yet most are optimized for general applications like air purification or solvent recovery, lacking the specific micropore tuning required for efficient aurocyanide complex capture.

PSD-GOLD fills this gap. Purpose-built for gold recovery circuits, it combines the inherent hardness and purity of premium coconut shell carbon with micropore engineering calibrated for rapid gold adsorption. The result: lower carbon fines, reduced gold losses to tailings, and consistent performance across multiple regeneration cycles—delivering the mining-grade reliability that general-purpose carbons cannot match.

  • Q
    What specific properties make PSD-GOLD ideal for gold recovery operations?
    A

    PSD-GOLD is manufactured from dense, mature coconut shells with high lignin content, delivering a robust granular structure for CIP, CIL, and CIC circuits. Its micropore architecture is tuned for rapid aurocyanide complex adsorption, while >98% hardness—the highest in the coconut shell range—minimizes fines generation during interstage screening. The result is high gold loading capacity, low attrition, and consistent performance in abrasive slurry environments.

  • Q
    How does PSD-GOLD minimize gold losses in recovery circuits?
    A

    Softer carbons generate excessive fines during pumping and screening; these fines escape interstage screens and carry adsorbed gold into tailings. PSD-GOLD’s >98% hardness resists mechanical breakdown under continuous slurry abrasion, drastically reducing fines generation. Less carbon loss means fewer gold particles reporting to tailings and lower carbon makeup costs.

  • Q
    What is the regenerability of PSD-GOLD after gold stripping?
    A

    PSD-GOLD supports efficient thermal reactivation. Its stable pore structure restores adsorption capacity across multiple regeneration cycles with minimal structural degradation. This multi-cycle regenerability reduces fresh carbon consumption and lowers operating costs in high-volume gold processing plants.

  • Q
    What mesh size is best for CIP/CIL/CIC gold recovery operations?
    A

    PSD-GOLD is available in 6×12 mesh and 4×8 mesh. The 6×12 mesh suits most CIP and CIL operations, balancing adsorption kinetics with screen separation efficiency. The 4×8 mesh is preferred for CIC systems where larger particles support solution flow dynamics. Both sizes maintain the same high hardness and gold-loading performance.

  • Q
    Why choose coconut shell carbon over wood or peat carbon for gold mining?
    A

    Wood and peat carbons suffer from significantly higher attrition in abrasive CIP/CIL slurries, generating fines that carry gold into tailings and inflate carbon losses. PSD-GOLD selects premium coconut shells with high lignin content and engineers the micropore structure specifically for aurocyanide adsorption, delivering the mining-grade hardness and recovery efficiency that softer carbons cannot match.

Free to contact us